X

Joining Dissimilar Materials

The welding robot machine for welding automotive part in the light blue scene.Industrial 4.0 concept for modern manufacturing process.

Multi-material design approach involves using High-Strength Steels and low-density materials, such as aluminium. The key idea is to utilize the right material for the right application in such a way that it should fulfill the service requirements and achieve mass efficiency at the same time. However, it is challenging to fully utilize multi-material design concepts due to joining issues.

Joining is considered a backbone of any manufactured assembly, since the ultimate reliability and integrity of the manufactured product relies on these joints. Dissimilar materials are difficult to join due to the difference in the physical and thermal properties. For example, one of the most desired combinations is aluminium to steel joints, which is challenging due to the large mismatch in the mechanical properties as shown in Table 1. This Joining section is dedicated specifically to the key joining issues between aluminium and steel.

Table 1:  Aluminium vs. Steel Material Mechanical Properties

Currently there are three approaches to joining dissimilar materials: solid-state joining, partial solid-state joining and arc joining. During solid state welding, the peak temperature of the process remains below the melting temperatures of the materials to be joined. Examples include diffusion bonding, ultrasonic welding, magnetic pulse welding, friction stir welding and vaporizing foil actuator welding. In partial solid-state welding processes, the peak temperature goes beyond the melting temperature of one of the materials to be joined (e.g. arc brazing & resistance spot welding). The last process (arc welding) has a peak temperature above the melting temperature of both materials to be joined. Practically it is not used anywhere however, it can be utilized in certain applications where the mismatch between the physical properties of the materials to be joined is little.

Among various joining processes, resistance spot welding (RSW) is one of the most widely used joining process in the automotive and aerospace industry due to its ease of automation and high productivity.  Browse the topics below to learn more about joining dissimilar materials.

 

 

 

Related Posts
Filter by
Post Page
Friction Stir Welding Mechanical Joining Adhesive Joining homepage-featured-top main-blog Steel Grades AHSS Blog Joining Joining Dissimilar Materials Resistance Welding Processes Resistance Spot Welding RSW of Dissimilar Steel RSW Modelling and Performance Tool & Die Professionals
Sort by

FSSW Method for Joining Ultra-Thin Steel Sheet

This article summarizes a paper entitled, “An Evaluation of Friction Stir Spot Welding as a Method for Joining

18

Mechanical Joining

Examples of mechanical joining in automotive manufacturing are clinching and self-piercing riveting. The process

18

Adhesive and Mechanical Joining

Fundamentals and Principles of Adhesive Joining Adhesive bonding is a joining process for metals and

18

AHSS Fundamentals in Forming and Joining

In this edition of AHSS Insights, George Coates and Menachem Kimchi get back to basics with important

18

Resistance Spot Welding with Advanced High-Strength Steels: Cold Stamped and Hot Formed

The discussions relative to cold stamping are applicable to any forming operation occurring at room temperature

8

Current Vehicle Examples

Manufacturers embrace Advanced High Strength Steels as a cost-effective way to satisfy functional and regulatory

8

Rationale

Automakers face conflicting constraints when designing new body structures: With escalating concerns

8

Resistance Spot Welding AHSS to Magnesium

This blog is a short summary of a published comprehensive research work titled:

8

Resistance Spot Welding: 5T Dissimilar Steel Stack-ups for Automotive Applications

Urbanization and waning interest in vehicle ownership point to new transport opportunities in megacities around the

8

Kate Hickey:
Related Post