J-21

Citation:

J-21. K. R. Jo, L. Cho, D. H. Sulistiyo, E. J. Seo, S. W. Kim and B. C. D. Cooman, “Effects of Al-Si coating and Zn coating on the hydrogen uptake and embrittlement of ultra-high strength press-hardened steel,” Surface and Coatings Technology, vol. 374, pp. 1108-1119, 2019, doi.org/10.1016/j.surfcoat.2019.06.047.

Related Posts
Filter by
Post Page
Press Hardened Steels Joining Laser Welding Arc Welding Coatings Solid State Welding Resistance Spot Welding main-blog homepage-featured-top Steel Grades AHSS Blog Joining Dissimilar Materials
Sort by

Role of Coatings in the Formation of Defects in AHSS Welds

A common issue when welding Advanced High-Strength Steels (AHSS) is with protective coatings causing weld defects. A

18

Coating Friction

Friction during the stamping process is a key variable which impacts metal flow. It

18

Coatings

topofpage

18

Effect GA-Coating Evolution PHS

This article summarizes a paper, entitled “Effect of GA-Coating Evolution during Press-Hardening on Fiber

18

Coating Effects

One of the methods by which the coatings are applied to the steel sheet surface is through a process called

18

AHSS Corrosion Resistant Coatings

Many steel parts on a vehicle require corrosion protection, regardless of whether they are exposed or unexposed

18

Resistance Spot Welding with Advanced High-Strength Steels: Cold Stamped and Hot Formed

The discussions relative to cold stamping are applicable to any forming operation occurring at room temperature

8

Categories: Citations
Angela Erhart:
Related Post