Citation:
C-28. L. Cho, H. Kang, C. Lee and B. C. D. Cooman, “Microstructure of liquid metal embrittlement cracks on Zn-coated 22MnB5 press-hardened steel,” Scripta Materialia, Vols. 90-91, pp. 25-28, 2014, doi.org/10.1016/j.scriptamat.2014.07.008.
C-28. L. Cho, H. Kang, C. Lee and B. C. D. Cooman, “Microstructure of liquid metal embrittlement cracks on Zn-coated 22MnB5 press-hardened steel,” Scripta Materialia, Vols. 90-91, pp. 25-28, 2014, doi.org/10.1016/j.scriptamat.2014.07.008.
H-66. G.T. Halmos (Editor) Roll Forming Handbook (1st ed.). CRC Press, 2005. doi.org/10.1201/9781420030693.
G.T. Halmos (Editor) Roll Forming Handbook (1st ed.). CRC Press, 2005.doi.org/10.1201/9781420030693
Citation U-13. Peter Ulintz, Precision Metalforming Association. This section originally appeared in the September 2023…