Citation:
B-65. B.-A. Behrens, A. Bouguecha, C. M. Gaebel, J. Moritz and J. Schrödter, “Hot Stamping of Load Adjusted Structural Parts,” Procedia Engineering, vol. 81, pp. 1756-1761, 2014, doi.org/10.1016/j.proeng.2014.10.227.
B-65. B.-A. Behrens, A. Bouguecha, C. M. Gaebel, J. Moritz and J. Schrödter, “Hot Stamping of Load Adjusted Structural Parts,” Procedia Engineering, vol. 81, pp. 1756-1761, 2014, doi.org/10.1016/j.proeng.2014.10.227.
H-66. G.T. Halmos (Editor) Roll Forming Handbook (1st ed.). CRC Press, 2005. doi.org/10.1201/9781420030693.
G.T. Halmos (Editor) Roll Forming Handbook (1st ed.). CRC Press, 2005.doi.org/10.1201/9781420030693
Citation U-13. Peter Ulintz, Precision Metalforming Association. This section originally appeared in the September 2023…