X

RSW of Dissimilar Steel

A variety of steel grades are used to manufacture vehicle body structures and closures. Welding dissimilar Advanced High-Strength Steels (AHSS) in three and four layer stack-ups requires special considerations. In this section of the Guidelines are articles summarizing papers that have investigated welding dissimilar AHSS and stack ups and discovered important factors for consideration and implementation.

Related Posts
Filter by
Post Page
Blog RSW Modelling and Performance RSW Parameter Guidelines RSW of Dissimilar Steel Resistance Spot Welding Joining Dissimilar Materials Resistance Welding Steel to Aluminium
Sort by

LME Simulation During RSW

Modern car bodies today are made of increasing volumes of Advanced High-Strength Steels (AHSS), the superb

18

RSW of 22MnB5 at Overlaps

This article summarizes a paper entitled, “RSW of 22MnB5 at Overlaps with Gaps-Effects, Causes, and

18

RSW of 3T Stack Up

This article is the summary of a paper entitled, “HAZ Softening of RSW of 3T Dissimilar Steel Stack-up”,

18

RSW Modelling Process and Performance

The advantages of numerical simulations for

18

Other RSW Considerations

Judging Weldability Using Carbon Equivalence (CE) Existing Carbon Equivalent (CE) formulas for Resistance

18

RSW of Advanced High-Strength Steels

In general, if any type of AHSS [

18

Ultrasonic Assisted RSW

Recently research at the Ohio State

18

Direct RSW of Aluminium to Steel

Figure 1 shows a typical cross-section of a

18

Key Issues: RSW Steel and Aluminium Joints

Among various dissimilar material combinations, Al-steel is one of the most desirable combination. This section will