Metallurgy of Mild Steels

Mild steels are low carbon steels with no alloying elements added for substantial strengthening, and for that reason are characterized by relatively lower yield strength. Typically, mild steels have less than 0.10% carbon.

These steels have a microstructure that is primarily ferrite. The amount of pearlite in the microstructure is a function of the amount of carbon in the steel, with lower carbon resulting in a lower fraction of pearlite. More information about microstructural components is available here.

Ultra-low carbon steels are a type of mild steel. These grades are typically the lowest yield strength and highest ductility available. Generally, these steels have less than 0.005% carbon, or less than 50 ppm C. More information is contained on the page for Ultra-Low Carbon steels.

Different names may describe mild steels, but these differences came from steel mill production techniques that are no longer in use. Since all sheet steels in use today are continuously cast, there are no significant differences between these terms:

  • Drawing Quality (DQ)
  • Drawing Steel (DS)
  • Aluminum Killed Drawing Quality (AKDQ)
  • Drawing Quality Aluminum Killed (DQAK)
  • Drawing Quality Special Killed (DQSK)

Mild steels are described in OEM, regional or global specifications with different syntax. While certain grade definitions between these specifications may be similar, the user is cautioned against using conversion charts without first confirming aspects which might be different, such as minimum, maximum, or typical values of chemical or mechanical properties. For example, ASTM specifications which cover lower strength steels list only typical values for tensile properties, but these are non-mandatory and the user may receive product outside the ranges shown. Additionally, JIS specifications which cover lower strength steels do not have minimum yield strength requirements, and the minimum elongation varies by thickness.

Some of the specifications describing uncoated cold rolled mild steel are included below, with the grades typically listed in order of increasing ductility. Different specifications may exist which describe hot or cold rolled, uncoated or coated, or steels of different strengths. Many automakers have proprietary specifications which encompass their requirements.

  • ASTM A1008M, with the terms CS, DS, DDS, and EDDSA-25
  • EN10130, with the terms DC01, DC03, DC04, DC05, and DC06D-3
  • JIS G3141, with the terms SPCC, SPCD, SPCE, SPCF, and SPCGJ-2
  • JFS A2001, with the terms JSC270C, JSC270D, JSC270E, JSC270F, and JSC260GJ-23
  • VDA239-100, with the terms CR1, CR2, CR3, CR4, and CR5V-3
Related Posts
Filter by
Post Page
Steel Grades AHSS 1stGen AHSS homepage-featured-top main-blog Blog Simulation Metallurgy Tailored Products Springback Cutting Cutting-Blanking-Shearing-Trimming
Sort by

Conventional Rule-of-Thumb Calculations Lead to Inaccurate Press Tonnage Predictions

The rule of thumb estimates used in 1989 during my internship with an automotive stamping supplier were simple

8

Servo Press Force and Energy Considerations When Working With AHSS

Advanced High-Strength Steel (AHSS) products have significantly different forming characteristics and these

8

A New Global Formability Diagram

Bubble chart. Banana diagram. Steel strength ductility diagram—it’s been called a lot of things over the years. But t

8

Additive Manufacturing

Additive Manufacturing (AM) has been associated with the future of manufacturing since its inception. While it does

8