Citation:
T-4. L. Tajul, T. Maeno, T. Kinoshita and K.-i. Mori, “Successive forging of tailored blank having thickness distribution for hot stamping,” The International Journal of Advanced Manufacturing Technology, vol. 89, pp. 3731-3739, 01 4 2017, doi.org/10.1007/s00170-016-9356-z.