Citation:

R-16R. Rana, “Special issue on ‘Medium manganese steels”, Materials Science and Technology, Volume 35, Issue 17, 2019, 2039-2044, doi.org/10.1080/02670836.2019.1673971.

Related Posts
Filter by
Post Page
Joining Dissimilar Materials Resistance Welding Steel to Aluminium Manufacturing Issues homepage-featured-top main-blog Blog Joining Resistance Welding Processes Resistance Spot Welding Arc Welding Automotive Welding Process Comparison resistance welding projection Steel Grades AHSS Forming Springback 3rdGen AHSS Roll Forming Roll Stamping Press Hardened Steels Production Managers Tool & Die Professionals 1stGen AHSS 2ndGen AHSS Citations Metallurgy Lower Strength Steels Conventional HSS
Sort by

Key Issues: RSW Steel and Aluminium Joints

Among various dissimilar material combinations, Al-steel is one of the most desirable combination. This section will

18

Four Steps to Mitigate Liquid Metal Embrittlement When Welding Steel

Liquid Metal Embrittlement (LME) during Resistance Spot Welding (RSW) can cause cracks when welding advanced

8

Resistance Spot Welding with Advanced High-Strength Steels: Cold Stamped and Hot Formed

The discussions relative to cold stamping are applicable to any forming operation occurring at room temperature

8

Stronger AHSS Knowledge Required for Metal Stampers

This month’s blog was contributed by

8

U-13

Citation U-13.

8

Key Issues: RSW Steel and Aluminium Joints

Among various dissimilar material combinations, Al-steel is one of the most desirable combination. This section will

18