M-56. J. Mola and B.C. De Cooman, “Quenching and partitioning processing of transformable ferritic stainless steels,” Scripta Materialia, Volume 65, Issue 9, 2011, Pages 834-837, doi.org/10.1016/j.scriptamat.2011.07.041. 