C-15. P.C.Chakraborti and M.K.Mitra, “Room temperature low cycle fatigue behaviour of two high strength lamellar duplex ferrite–martensite (DFM) steels,” International Journal of Fatigue, Volume 27, Issue 5, May 2005, Pages 511-518; doi.org/10.1016/j.ijfatigue.2004.09.003.
Normal vehicle use leads to repeated loading of components and joints. Stress concentrations in the body structure
18
Using Life Cycle Assessment to Determine Steel E-Motive Concept Vehicle Emissions
The transportation industry’s contribution to greenhouse gas (GHG) emissions and global warming is well d