B-45. E. Billur, G. Berglund and T. Gustafsson, “History and Future Outlook of Hot Stamping,” in “Hot stamping of ultra high-strength steels: From a Technological and Business Perspective,” edited by E. Billur, Springer, 2019, pages 31-44; 