G-29
Citation:
G-29. I. M. Gonzales and O. Straube, “Development of Zinc Coated Parts for Hotstamping,” in Proceedings of New Developments in Sheet Metal Forming Conference, Stuttgart, Germany, 2016;
G-29. I. M. Gonzales and O. Straube, “Development of Zinc Coated Parts for Hotstamping,” in Proceedings of New Developments in Sheet Metal Forming Conference, Stuttgart, Germany, 2016;
C-17. M. R. de Castro, W. A. Monteiro and R. Politano, “Enhancements on strength of body structure due to bake hardening effect on hot stamping steel,” The International Journal of Advanced Manufacturing Technology, vol. 100, pp. 771-782, 01 1 2019, doi.org/10.1007/s00170-018-2542-4;
J-17. H. Järvinen, M. Honkanen, M. Järvenpää and P. Peura, “Effect of paint baking treatment on the properties of press hardened boron steels,” Journal of Materials Processing Technology, vol. 252, pp. 90-104, 2018, doi.org/10.1016/j.jmatprotec.2017.08.027.
V-10. L. Vaissiere, J. P. Laurent and A. Reinhardt, “Development of Pre-Coated Boron Steel for Applications on PSA Peugeot Citroën and Renault Bodies in White“, SAE Technical Paper 2002-01-2048, 2002, saemobilus.sae.org/content/2002-01-2048.
M-25. H. Mohrbacher, “Martensitic Automotive Steel Sheet – Fundamentals and Metallurgical Optimization Strategies“, Advanced Materials Research, 1063, 130–142, 2014, doi.org/10.4028/www.scientific.net/amr.1063.130.