Citation:
S-59. D.J. Schaeffler and E.J. Vineberg, “Troubleshooting Formability Problems Using Strain Analysis”, ASM Handbook, Volume 14B, Metalworking: Sheet Forming, ASM International, 2006, doi.org/10.31399/asm.hb.v14b.9781627081863.
S-59. D.J. Schaeffler and E.J. Vineberg, “Troubleshooting Formability Problems Using Strain Analysis”, ASM Handbook, Volume 14B, Metalworking: Sheet Forming, ASM International, 2006, doi.org/10.31399/asm.hb.v14b.9781627081863.
H-66. G.T. Halmos (Editor) Roll Forming Handbook (1st ed.). CRC Press, 2005. doi.org/10.1201/9781420030693.
G.T. Halmos (Editor) Roll Forming Handbook (1st ed.). CRC Press, 2005.doi.org/10.1201/9781420030693
Citation U-13. Peter Ulintz, Precision Metalforming Association. This section originally appeared in the September 2023…