Citation:
H-20. B. M. Hance and L. Huang, “A simplified stress-based forming limit criterion for advanced high strength steel (AHSS),” IDDRG 2018, 2018 IOP Conf. Ser.: Mater. Sci. Eng. 418 012037, doi:10.1088/1757-899X/418/1/012037 .
H-20. B. M. Hance and L. Huang, “A simplified stress-based forming limit criterion for advanced high strength steel (AHSS),” IDDRG 2018, 2018 IOP Conf. Ser.: Mater. Sci. Eng. 418 012037, doi:10.1088/1757-899X/418/1/012037 .
H-66. G.T. Halmos (Editor) Roll Forming Handbook (1st ed.). CRC Press, 2005. doi.org/10.1201/9781420030693.
G.T. Halmos (Editor) Roll Forming Handbook (1st ed.). CRC Press, 2005.doi.org/10.1201/9781420030693
Citation U-13. Peter Ulintz, Precision Metalforming Association. This section originally appeared in the September 2023…