M-27
Citation:
M-27. Mercedes-Benz, “DBL4093: Body parts manufactured from press-hardened steel sheets,” Company Standard , 2017.
M-27. Mercedes-Benz, “DBL4093: Body parts manufactured from press-hardened steel sheets,” Company Standard , 2017.
V-11. voestalpine Stahl GmbH, “Data sheet phs-ultraform®“, 08/2018, 2018.
T-28. ThyssenKrupp Steel Europe AG, “Product information for manganese-boron steel for hot forming,” Product Catalogue, June 2020.
P-21. A. Pic and F. Pinard, “Usibor ® and Ductibor®: a “hot” combination for safer and lighter cars”, ArcelorMittal Update, p. 12–13, 2009.
T-27. B. Tang, Z. Yuan, G. Cheng, L. Huang, W. Zheng and H. Xie, “Experimental verification of tailor welded joining partners for hot stamping and analytical modeling of TWBs rheological constitutive in austenitic state,” Materials Science and Engineering: A, vol. 585, pp. 304-318, 2013, doi.org/10.1016/j.msea.2013.07.059.