Citations
Citation:
D-31. F. D’Aiuto, “Innovative materials and solutions for automotive components,” Presented at ANFIA – Associazione Nazionale Fra Industrie Automobilistiche (National Association of the Automobile Industry; Torino, Italy), 28 April 2016.
Citations
Citation:
N-24. Jae-Bok Nam, “Development of New Auto Steels and Application Technology,” worldsteel / CISA China Automotive Steel Conference, Nov. 21, 2013
Citations
Citation:
C-30. P. Cugy, A. Hildenbrand, M. Bouzekri, D. Cornette, S. Göklü, and H. Hofmann, “A Super-High Strength Fe-Mn-C Austenitic Steel with Excellent Formability for Automobile Applications,” 2005;
Citations
Citation:
D-30. B.C. De Cooman, O. Kwon, and K.-G. Chin, “State-of-the-knowledge on TWIP steel,” Materials Science and Technology, Volume 28, Number 5, 2012, pages 513-527, doi.org/10.1179/1743284711Y.0000000095.
Citations
Citation:
K-42. S.-K. Kim, G. Kim, and K.-G. Chin, “Development of High Manganese TWIP Steel with 980MPa Tensile Strength,” International Conference on New Developments in Advanced High-Strength Sheet Steels, 2008, Paper PR- 256-024, Page 249.