Welcome to AHSSInsights.org, the leading online resource for technical information on the forming, joining and metallurgy of Advanced High-Strength Steels for automotive applications.
This site features a searchable database, enabling easy access to critical information on the key benefits of automotive high strength steels and how they can be deployed for manufacture. The content is made publicly available by WorldAutoSteel, the automotive group of the World Steel Association.
Servo Press Force and Energy Considerations When Working With AHSS
Advanced High-Strength Steel (AHSS) products have significantly different forming characteristics and these challenge conventional mechanical and hydraulic presses. Some examples include the...
A New Global Formability Diagram
Bubble chart. Banana diagram. Steel strength ductility diagram—it’s been called a lot of things over the years. But the 2021 chart shown in Figure 1 is the subject of hundreds of requests for use we...
Additive Manufacturing
Additive Manufacturing (AM) has been associated with the future of manufacturing since its inception. While it does hold several advantages in complex geometries and low-volume production, modern AM...
Vision for Industry 4.0 in Sheet Metal Forming
There is interest in the sheet metal industry on how to adopt Industry 4.0 into their legacy forming practices to significantly improve productivity and product quality. Figure 1 illustrates four...
Welcome to the All New AHSS Application Guidelines!
The leading source for technical best practices on the forming and joining of Advanced High-Strength Steels (AHSS) for vehicle manufacture is released today by WorldAutoSteel, the automotive group...
Steel Structures for Autonomous Vehicles