L-61
Citation:
L-61. J. Lucas, “2021 Acura TLX“, Presented at 2021 Great Designs in Steel, Sponsored by American Iron and Steel Institute.
L-61. J. Lucas, “2021 Acura TLX“, Presented at 2021 Great Designs in Steel, Sponsored by American Iron and Steel Institute.
F-42. R. Funada, “Maximizing Lightweighting in Steel Automotive Bodies and Frames with STAF (Steel Tube Air Forming)“, Presented at 2021 Great Designs in Steel, Sponsored by American Iron and Steel Institute.
L-60. Q. Lu, S. Tedesco, M. Shi, J. Coryell, and J. Wang, “New Generation Oxidation Resistance (Coating Free) Press Hardening Steel”, Presented at 2021 Great Designs in Steel, Sponsored by American Iron and Steel Institute.
K-56. H. Kim, J. Gu, M. Enloe, and J. P Singh, “A New Testing Method For Evaluating Edge Cracking Of AHSS“, Presented at 2021 Great Designs in Steel, Sponsored by American Iron and Steel Institute.
Z-15. D.J. Zhou, and K. Kannan, “The Effect of Combination Beads on Springback: Experimental Study & Virtual Study“, Presented at 2021 Great Designs in Steel, Sponsored by American Iron and Steel Institute.