S-121
Citations:
S-121. J. Staudte, J. M. Mataigne, F. Del Frate, D. Loison and S. Cremel, “Optimizing the manganese and silicon content for hot dip galvanizing of 3rd generation advanced high strength steels,” Metallurgical Research & Technology, Volume 111, Number 1, 2014, Pages 17 – 23; https://doi.org/10.1051/metal/2014003