L-2
Citation:
L-2. S. Lalam, B. Yan, “Weldability of AHSS,” Society of Automotive Engineers, International Congress, Detroit (2004).
L-2. S. Lalam, B. Yan, “Weldability of AHSS,” Society of Automotive Engineers, International Congress, Detroit (2004).
T-6. M. Tumuluru, “A Comparative Examination of the Resistance Spot Welding Behavior of Two Advanced High Strength Steels,” SAE Paper 2006-01-1214, 2006, doi.org/10.4271/2006-01-1214.