N-16

Citation:

N-16. R. Neugebauer, M. Werner, A. Paul and F. Schieck, “Media based press hardening of tubes—opportunities and challenges,” Proceedings of the 5th International Conference on Tube Hydroforming, edited by Kenichi Manabe, Japan Society for Technology of Plasticity, Noboribetsu, 2011.