J-22. R. Johansson, M. Fermer, J. Jergeus and J. K. Larsson, “Extensive Use of Hot-Formed Steel in Car Body Structures,” in 3rd International Conference on Hot Sheet Metal Forming of High Performance Steel, CHS2, Kassel, Germany, 2011.