C-18
Citation:
C-18. J. T. Cantrell, S. Rohde, D. Damiani, R. Gurnani, L. DiSandro, J. Anton, A. Young, A. Jerez, D. Steinbach, C. Kroese, and P. G. Ifju, “Experimental characterization of the mechanical properties of 3D-printed ABS and polycarbonate parts,” Rapid Prototyping Journal, Vol. 23 No. 4, pp. 811-824. doi.org/10.1108/RPJ-03-2016-0042;