O-11
Citation:
O-11. M. Oldenburg, “Simulation Methods for Press Hardening Applications,” Tutorial presented at 5th Intl. Conference on Hot Sheet Metal Forming of High Performance Steel, CHS2, June 2nd, Toronto, ON, Canada, 2015.
O-11. M. Oldenburg, “Simulation Methods for Press Hardening Applications,” Tutorial presented at 5th Intl. Conference on Hot Sheet Metal Forming of High Performance Steel, CHS2, June 2nd, Toronto, ON, Canada, 2015.
E-7. M. Eriksson, M. Oldenburg, M.C. Somani, and L.P. Karjalainen, “Testing and Evaluation of Material Data for Analysis of Forming and Hardening of Boron Steel Components,” Modelling and Simulation in Materials Science and Engineering, Volume 10, Number 3, 2002, pp. 277–294, doi.org/10.1088/0965-0393/10/3/303;