H-36
Citation:
H-36. J. Heingärtner, P. Fischer, D. Harsch, Y. Renkci, and P. Hora, “Q-Guard – an intelligent process control system”, Presented at International Deep Drawing Research Group – 2017, IOP Conf. Series: Journal of Physics: Conf. Series 896 (2017) 012032, doi.org/10.1088/1742-6596/896/1/012032.