Citations
Citation:
M-29. N. Mahayotsanun, S. Sah, J. Cao, M. Peshkin, R. X. Gao, and C. Wang, “Tooling-integrated sensing systems for stamping process monitoring,” International Journal of Machine Tools and Manufacture, Volume 49, Issues 7–8, 2009, Pages 634-644, doi.org/10.1016/j.ijmachtools.2009.01.009.
Citations
Citation:
A-57. J.M. Allwood, S.R. Duncan, J. Cao, P. Groche, G. Hirt, B. Kinsey, T. Kuboki, M. Liewald, A. Sterzing, and A.E. Tekkaya, “Closed-loop control of product properties in metal forming,” CIRP Annals, Volume 65, Issue 2, 2016, Pages 573-596, doi.org/10.1016/j.cirp.2016.06.002.
Citations
Citation:
Y-13. D.Y. Yang, M. Bambach, J. Cao, J.R. Duflou, P. Groche, T. Kuboki, A. Sterzing, A.E. Tekkaya, and C.W. Lee, “Flexibility in metal forming“, CIRP Annals, Volume 67, Issue 2, 2018, Pages 743-765, doi.org/10.1016/j.cirp.2018.05.004.