V-25

Citations:   V-25.  VDA 238-110, “Ermittlung der Lokalen Duktilität aus der Bruchfläche von Zugproben / Determination of Local Ductility by Fracture Surface Analyses of Tensile Test Specimens 08/2023)),” Verband der Automobilindustrie e. V. (VDA),...

read more

L-72

Citations:   L-72.   LINGBEEK Roald, LAROUR Patrick, RUCK Astrid, BEIER Thorsten, CORNETTE Dominique, SCHADOW Thomas, WESTHÄUSER Sebastian, “Local ductility in steel sheet, towards a practical and robust measurement method,” Materials Research...

read more

S-128

Citations:   S-128.   SAE J2334, “Laboratory Cyclic Corrosion Test (Stabilized Apr 2016),” SAE International, 2016; https://www.sae.org/standards/content/j2334_201604/  

read more

V-6

Citations:   V-6.  VDA 233-102, “Zyklische Korrosionsprüfung von Werkstoffen und Bauteilen im Automobilbau / Cyclic corrosion testing of materials and components in automotive construction (Version 06/2013),” Verband der Automobilindustrie e. V. (VDA), 2013;...

read more

R-31

Citations:   R-31.  Arjan Rijkenberg, Toni Chezan, Maxim Aarnts, Sabri Sengo, Menno De Bruine, Carolien Heij-Verschoor, Bert Schouws, Brian Du Pont, Leen Visser, Ferry Zwanenburg, Ton De Boer, "The Relationship Between Hole-Expansion Capacity and Fracture...

read more

R-30

Citations:   R-30.  Arjan Rijkenberg, Toni Chezan, and Arnoud de Vooys, “Leveraging Fracture Toughness and Corrosion Resistance in the Development of Advanced High-Strength Steels for Automotive Chassis and Frame Applications,” International Automotive Body...

read more

A-93

Citations:   A-93.  Eisso Atzema, Petra Seda and Nico Langerak, “SETi, Sheared Edge Tensile test improved,” IDDRG 2015 Conference, May 31-June 03, 2015, Shanghai, China, https://iddrg.com/wp-content/uploads/2022/03/C_91_15.pdf  

read more

A-92

Citations:   A-92.  Eisso Atzema and Petra Seda, “Sheared Edge Tensile Test Improved: SETi,” Forming Technology Forum 2015, June 29 & 30, 2015, Zurich, Switzerland; available on page 97 in...

read more

S-127

Citations:   S-127.  Matthias Schneider, Thorsten Beier, Patrick Larour, Eisso Atzema, Matti Teschner, Sebastian Westhäuser, Martin Bülter, Michael Braun, Thomas Müller, Arno Richter, and Stefanie Brockmann, “Consideration of the reduced formability of a...

read more

C-45

Citations:   C-45.   A. Carley-Clopton, "Aging effects on sheared edge formability," Thesis, 2023, Colorado School of Mines; https://hdl.handle.net/11124/178651   