K-16
Citation:
K-16. H. Kim, J. Gu, M. Enloe, and J. P Singh, “Evaluations of Edge Formability for DP780 Materials from Different Suppliers,” Presented at the International Deep Drawing Research Group (IDDRG) conference, 2020.
K-16. H. Kim, J. Gu, M. Enloe, and J. P Singh, “Evaluations of Edge Formability for DP780 Materials from Different Suppliers,” Presented at the International Deep Drawing Research Group (IDDRG) conference, 2020.
H-20. B. M. Hance and L. Huang, “A simplified stress-based forming limit criterion for advanced high strength steel (AHSS),” IDDRG 2018, 2018 IOP Conf. Ser.: Mater. Sci. Eng. 418 012037, doi:10.1088/1757-899X/418/1/012037 .
D-17. Deutsches Institut fur Normung E.V. (DIN) Euronorm (EN), DIN EN 10268, “Cold rolled steel flat products with high yield strength for cold forming – Technical delivery conditions“.
F-10. M. Feistle, I. Pätzold, R. Golle, W. Volk, A. Frehn, and R. Ilskens, “Maximizing the Expansion Ratio through Multi-stage Shear-cutting Process during Collar Forming,” IOP Conference Series: Materials Science and Engineering, 418, 1, 012071, 10.1088/1757-899X/418/1/012071, 2018.
C-13. J.J. Coryell, “Edge Fracture in Mixed Microstructure Steels“, Presented at 2016 Great Designs in Steel, Sponsored by American Iron and Steel Institute.
S-53. H.-C. Shih and G. Hsiung, “Optimal Production Trimming Process For AHSS Edge Stretchability Improvement“, Presented at 2014 Great Designs in Steel, American Iron and Steel Institute.