image/svg+xml
0246810121416
02004006008001000120014001600
EngineeringStrain(e)[%]
EngineeringStress(σe)[MPa]
Corelayer: PHS1500 (22MnB5)
Outer layer: PQS450
Composite:Tribond® 1200
Prepared by Eren Billur, Billur Metal Formfor WorldAutoSteel AHSS Guidelines, 2021