image/svg+xml
0.010.11101001000
0100200300400500600
Coolingrate[°C/s]
VickersHardness[HV]
1.4006AISI SS410>1
°
C/s
100% MartensiteMartensite + Other Phases
22MnB5, >27
°
C/s
-0.200.20.4
00.10.20.30.40.5
MinorStrain[-]
MajorStrain[-]
DP6001.6065(modified AISISS410)
(a)
(b)
Prepared by Eren Billur, Billur Metal Formfor WorldAutoSteel AHSS Guidelines, 2021