image/svg+xml
0
100
200
300
400
500
600
700
800
900
0
100
200
300
400
500
600
700
800
Heating Temperature (T) [ ° C]
Tensile Strength ( σ UTS or R m ) [MPa]
0
200
400
600
800
1000
0
20
40
60
80
100
120
140
160
Total Elongation (A) [%]
0
100
200
300
400
500
600
700
800
900
0
100
200
300
400
500
600
700
800
Heating Temperature (T) [ ° C]
Tensile Strength ( σ UTS or R m ) [MPa]
0
200
400
600
800
1000
0
20
40
60
80
100
120
140
160
Total Elongation (A) [%]
PHS150022MnB5
1.4028 (AISI SS420F)Stainless
(a)
(b)
Prepared by Eren Billur, Billur Metal Formfor WorldAutoSteel AHSS Guidelines, 2021