image/svg+xml
0510152025
0500100015002000
EngineeringStrain(e)[%]
EngineeringStress(σe)[MPa]
PHS1500 as delivered
PHS1500 Full Hardened (FH)
PHS1500+GIasreceived(optimizedforcoldforming)
Prepared by Eren Billur, Billur Metal Formfor WorldAutoSteel AHSS Guidelines, 2021