image/svg+xml(a)(b)Hard ZoneHardness:400-520 HVYieldStrength:1000-1250 MPaUTS:1300-1650 MPaBendAngle: 546SoftZoneHardness:185-220 HVYieldStr.:450-550 MPaUTS:600-700 MPaBendAngle: 953Hard ZoneYieldStr.: 1100 MPaUTS: 1450 MPaA5:>6%SoftZoneYieldStr.: 400 MPaUTS: 550 MPaA5:>20%