Metallurgy of Ultra-Low Carbon Steels (DDS – EDDS)

ULC, IF, VD-IF, and EDDS are interchangeable terms that describe the most formable (high n-value) and lowest strength grade of steel.

Ultra-low-carbon (ULC) steels typically carbon levels less than 0.005%, or 50 parts per million.  At these low alloying levels, the atomic structure is primarily iron, with unfilled spaces or gaps (called interstices) between the atoms – the origin of the term “interstitial-free” or IF.  Molten steel needs an additional process prior to casting called vacuum degassing (VD) to reach these carbon levels.   Because this steel alloy is mainly iron and all pure elements are very formable, it is also referred to as either deep drawing steel (DDS) or extra-deep-drawing steel (EDDS).  Specifications which contain ULC grades are listed within the Mild Steels page.

Adding phosphorus to an IF grade increases the strength due to solid solution strengthening, precipitation of carbides and/or nitrides, and grain refinement. These higher strength IF-HS grades are widely used for both structural and closure applications.  Work hardening from forming will increase panel strength, and is sometimes called a dent resistant steel grade.  However, this alloying approach is not capable of producing a bake hardenable grade.

Related Posts
Filter by
Post Page
Friction Stir Welding Joining Dissimilar Materials Resistance Welding Steel to Aluminium General main-blog Metallurgy Steel Grades AHSS Blog 3rdGen AHSS homepage-featured-top Roll Forming Citations
Sort by

FSSW Method for Joining Ultra-Thin Steel Sheet

This article summarizes a paper entitled, “An Evaluation of Friction Stir Spot Welding as a Method for Joining

18

Steel E-Motive: Autonomous Vehicles That Only Steel Can Make Real

The Steel E-Motive program–commissioned by WorldAutoSteel in partnership with Ricardo plc–has developed the world’s f

8

L-64

Citation L-64. J.-S. Lee, “

8

More Reveals of the Steel E-Motive Autonomous Vehicle Demonstration

WorldAutoSteel has a 30-year legacy of steel demonstration all the way back to the

8

What are 3rd Gen AHSS?

One of the tasks we took great care in completing during the update of the AHSS Application Guidelines was to

8

Process, Microstructure and Fracture Mode of Thick Stack-Ups of Aluminum Alloy to AHSS Dissimilar Spot Joints

This article summarizes a paper entitled, “Process, Microstructure and Fracture Mode of Thick Stack-Ups of

8

A New Global Formability Diagram

Bubble chart. Banana diagram. Steel strength ductility diagram—it’s been called a lot of things over the years. But t

8